Shield-Bright 410NiMo

ESAB's new Shield-Bright 410NiMo is an all-position, gas-shielded, flux-cored electrode designed for the fabrication and repair of hydroelectric turbine runners and related components. Shield-Bright 410NiMo features a spray-like transfer that enhances the arc characteristics while minimizing post-weld clean up and rework. Shield-Bright 410 is easy to use and delivers consistent quality welds.

Click here to visit the Shield-Bright 410NiMo product page.

 