Florence, SC – ESAB Welding & Cutting Products has added two additional wires to its popular Dual Shield X-Series flux cored wires. The X-Series wires are more forgiving than traditional flux cored wires, especially for less experienced welders, with an easily controlled arc and improved operation at both lower and higher current levels. Dual Shield X wires also offer high deposition rates, fast travel speeds, flat bead profile, limited spatter and extremely easy slag removal for overall productivity, ease of use and outstanding operator appeal.

Dual Shield 810X-Ni1 is an all-position 1% Nickel flux cored wire for general purpose welding of low alloy steel. Dual Shield 810X-Ni1 is designed for use with 100% CO2 and is an excellent choice for welding on CORTEN steel in applications where weathering grade wires are not desirable. Common applications include power transmission, bridges, shipbuilding, railroad cars, barges, light equipment/heavy structural and general fabrication. This wire meets AWS A5.29; E81T1-Ni1C classifications, is certified by C.W.B. - CSA W48 and is certified for seismic applications.

Dual Shield 710X-M is an all-position flux cored wire for general purpose welding of mild steel. Dual Shield 710X-M is designed to be used with a 75/25 Argon/CO2 gas mix, however pure CO2 may also be used. Typical applications include railroad cars, shipbuilding, barges, light equipment, civil construction and general fabrication. Classifications and approvals include AWS A5.20; E71T-1C-D/T-9C-D; AWS A5.20; E71T-1M/T-9M; ASME SFA 5.20; A.B.S., and C.W.B. - CSA W48. This wire is certified for seismic applications.

With more than 100 years of experience, ESAB Welding & Cutting Products is one of the world’s largest and most skilled manufacturers of welding and cutting equipment and welding filler metals. Ensuring customer satisfaction, a wide range of ESAB products carry the 100% Satisfaction Guarantee. Recognized as the technological leader in the industry, ESAB is committed to providing customized solutions for their customers. For more information on the new Dual Shield X-Series wires, visit www.esabx.com or www.dualshieldx.com or call 1-800-ESAB123

DualshieldX_Wire_BlkBox_web
Powered by CommonSpot