No matter which of the four feeders you choose, it can be combined with any of the three new switching converter (chopper) power sources. With proven technology and ESAB-developed software, these choppers provide reliable, productive welding performance. Each unit is constructed with a strong metal casing to withstand harsh environments. The large wheels, sturdy lifting eyelets, and an undercarriage designed for transport by forklift make the unit easy to move. A dust filter handles tough and dirty environments, and prevents grinding dust and metal particles from entering the chassis (optional). All you have to decide is how much power you need.

MIG 4002c MIG 5002c MIG 6502c
Mains voltage 230/460 V 3 ph 60 Hz 230/460 V 3 ph 60 Hz 230/460 V 3 ph 60 Hz
Permitted load at 60% duty cycle 400 A / 34 V 500 A / 39 V 650 A / 44 V
Permitted load at 100% duty cycle 310 A / 30 V 400 A / 34 V 500 A / 39 V
Primary current at 60% duty cycle 56/26 A 75/34 A 103/47 A
Primary current at 100% duty cycle 43/20 A 57/26 A 80/37 A
Setting range (DC) GMAW/FCAW (MIG/MAG) 16-400 A / 8-60 V 16-500 A / 8-60 V 16-650 A / 8-60 V
Setting range (STICK) 16-400 A 16-500 A 16-650 A
Open circuit voltage GMAW/FCAW (MIG/MAG) 62 V 62 V 62 V
Open circuit voltage SMAW (STICK) 68 V 68 V 68 V
Open circuit power 500 W 550 W 670 W
In energy saving mode, 15 min. after welding 60 W 60 W 60 W
Power factor at maximum current 0.88 0.90 0.90
Efficiency at maximum current 70% 72% 76%
Control voltage 42 V, 50/60 Hz 42 V, 50/60 Hz 42 V, 50/60 Hz
Dimensions L x W x H 32.6 x 25.1 x 32.8 in.
(830 x 640 x 835 mm)
32.6 x 25.1 x 32.8 in.
(830 x 640 x 835 mm)
32.6 x 25.1 x 32.8 in.
(830 x 640 x 835 mm)
Weight 328 lb (149 kg) 407 lb (185 kg) 489 lb (222 kg)
Weight with cooling unit 359 lb (163 kg) 438 lb (199 kg) 520 lb (236 kg)
Operating temperature 14 to 104°F (-10 to 40°C) 14 to 104°F (-10 to 40°C) 14 to 104°F (-10 to 40°C)
Enclosure class IP 23 IP 23 IP 23