The new Falcon CXL is ESAB's newest gantry for oxy-fuel and plasma cutting or oxy-fuel/plasma combination. The system features ESAB's m3 Precision Plasmarc system, which allows the machine to cut and mark with the same plasma torch. The Falcon CXL is available in 200 Amp or 360 Amp configurations. Depending on the configuration, the system can cut carbon steel up to 2.5 in. (63.5 mm) thick, or stainless steel up to 1.5 in. (38 mm) thick and aluminum up to 1.75 in. (44.5 mm) thick. With many standard features included, the Falcon CXL comes shipped ready to work!