Self-Shielded
Flux
Cored Arc Welding (FCAW-S)
Semiautomatic
Short
Circuit Gas
Metal Arc Welding
(GMAW-S)
Spatter
Standoff
Distance
Stickout
Stub
A flux cored arc welding process variation in which shielding gas is obtained
exclusively from the flux within the electrode.
Pertaining to the manual control of a process with equipment that automatically
controls one or more of the process conditions.
A gas metal arc welding process variation in which the consumable electrode
is deposited during repeated short circuits.
Weld
reinforcement opposite the side from which welding was done.
The distance between a nozzle and the workpiece.
The
length of unmelted electrode extending beyond the end of the gas nozzle.
ABCD
- EFGH
- IJ
- KLMN
- O
P
Q
- R
S
T
U
- V
W
- X
Y - Z
The
short length of filler metal electrode, welding rod, or brazing rod that remains
after its use for welding or brazing.