18
HORIZONTAL POSITION
Recommended weaving patterns, torch
positions and bead sequences are shown in Figure 7-16. For fillet
welds, a circular motion is recommended.
For butt weld root passes and fill passes, an in-line, back-and-
forth motion is used with width adjustments
as required. A slight pause is used at the tie-in to the previous
bead. Figure
7-16 - Torch Manipulations