4 Typical
Mechanical Properties As
Welded Yield Strength,
psi (MPa) 91,500
(631) Tensile
Strength, psi (MPa) 101,750
(702) %
Elongation in 2" (51 mm) 24
% Reduction in Area
64 Hardness
29 Rc* *Two
Layers weaving on 1020 Steel Weld
deposits can be cut with oxy-acetylene torch or by air carbon-arc cutting.
Typical Undiluted Weld Metal Analysis
(%) C
Mn Si
Cr Mo
0.20 Max. 0.09
0.70 2.30
1.10 Properties
of Deposited Weld Metal: The
chromium and molybdenum alloy balance imparts impact and compression resistance,
as well as considerable
wear resistance to the weld metal in all thicknesses of buildup.
Standard Diameters
1/8" (3.2 mm), 5/32" (4.0 mm), 3/16"