4 Voltage Sensitivity                      Weld Metal Unionmelt Spoolarc Recommended Max. Base Metal Flux Wire Volts Mn (%) Si (%) Thickness in. (mm) 231 81 28 1.54 0.68 1 (25) 35 1.90 1.04 1 (25) 350 81 28 1.27 0.56 1 (25) 35 1.53 0.79 1 (25) 429 81 28 1.32 0.51 Unlimited 35 1.45 0.55 Unlimited 439 81 28 1.30 0.24 Unlimited 36 1.46 0.25 Unlimited 651VF 81 28 0.85 0.35 Unlimited 36 0.91 0.39 Unlimited 656 81 28 1.26 0.16 Unlimited 35 1.24 0.13 Unlimited