4 Spoolarc
65 AWS Class ER70S-2
Code and Specification Data:
AWS A5.18, ASME SFA 5.18
Military - MIL 70S-2, MIL-E-23765/1
ABS - ER70S-2 CWB-CSA
W48.4-M, ER480S-2 Description:
Spoolarc 65 is a triple deoxidized (aluminum,
titanium, zirconium) welding wire designed for welding over
rust and mill scale. The less fluid
weld puddle of Spoolarc 65 makes it easy to control when used out of
position. Spoolarc
65 is the preferred wire for all position welding of small diameter pipe. This
product is available in forms
suitable for MIG and TIG welding. Typical
Mechanical Properties As
Welded GMAW
GTAW Testing
Temp. 98% Ar/2%
O2 CO2
Argon Yield
Strength, psi (MPa) 68,000 (469)
70,700 (487)
67,500 (466)
Tensile Strength, psi (MPa)
82,000 (566)
80,000 (552)
77,500 (534)
% Elongation in 2" (51 mm)
28 26
31 Continued
on next page...