3 Carbon
Steel Wires Spoolarc
Easy Grind No AWS
Class Description:
Spoolarc Easy Grind is a fully deoxidized
wire designed to weld over moderate levels of rust and paint as
are commonly encountered in auto body
repair work. Easy Grind produces welds that easily meet the tensile
requirements of other ER70S class wires.
Easy Grind is produced in small diameters
and is appropriate for the low current welding machines commonly
used in body shops. Typical
Mechanical Properties As
Welded 75% Ar/25%
CO2 Yield
Strength, psi (MPa) 72,000
(497) Tensile
Strength, psi (MPa) 80,000
(552) %
Elongation in 2" (51 mm) 24
Typical Charpy V-Notch Impact Properties
As Welded Testing
Temp. ft.-lbs.
(J) -20°F(-29°C)
40 (54)
Standard Diameters
.023" (0.6 mm), .030" (0.8 mm)
Recommended Welding Parameters pages
27 & 28