43 Typical Undiluted Typical Mechanical Weld Metal Analysis Type Properties % wt Specifications 75/25   75/25    (CO2) Shield-Bright X-tra 316L AWS A5.22 Tensile Strength C 0.03 (0.03) ASME SFA 5.22 82,800 psi (571 MPa) Mn 1.6 (1.5) Class Yield Strength Si 0.7 (0.6) E316LT0-1/T0-4 63,100 psi (435 MPa) Cr 19.0 (18.8) MIL-Conf. A5.22 % Elongation in 2" (51 mm) Ni 12.0 (12.0) CWB, TUV 37 Mo 2.6 (2.5) ABS-A5.22 FN 9 (7.5) Designed specifically for applications where the service environment can produce pitting corrosion. Commonly used in the pulp and paper industry. Shield-Bright X-tra 317L AWS A5.22 Tensile Strength C 0.03 (0.03) ASME SFA 5.22 89,500 psi (618 MPa) Mn 1.5 (1.4) Class Yield Strength Si 0.6 (0.5) E317LT0-1/T0-4 69,000 psi (476 MPa) Cr 19.5 (19.4) % Elongation in 2" (51 mm) Ni 12.5 (12.6) 34 Mo 3.5 (3.5) FN 10 (9) For  welding type 317 and 317L stainless where additional corrosion resistance that type 316L cannot provide. Continued on next page...
Electrodes
Covered
Stainless
Steel
Products
Solid Wire
& Rod
Products
ESAB
TIG & MIG
Wires
Cored
Wire
Products
Submerged
Arc
Products
Hard-
surfacing
Products
Calculations
Filler Metals
ASTM
Steels
Conversion
Tables
Arcaloy SS
Electrode Coat.
Arcaloy
Bare Wires
Arcaloy Metal
Core Wires
Nickel-Arc/
Nicore Cast Iron
Shield-Bright
Gas/Flux Cored
Core-Bright
Cored Wires