20 Typical Undiluted Type Weld Metal Analysis Specifications % wt Arcaloy ER347 AWS A5.9 Carbon 0.06 ASME SFA 5.9 Manganese 1.8 Class ER347 Silicon 0.4 MIL-19933 Chromium 20.0 MIL-347 Nickel 9.8 Niobium 0.8 FN 8 For welding types 304, 321 and 347, when the service temperature is below 600°F (316°C). Additional Arcaloy Stainless Steel Bare Wires* Arcaloy ER308H (ER308/308H) Arcaloy ER310 (ER310) Arcaloy ER312 (ER312) Arcaloy ER316H (ER316/316H) Arcaloy ER320LR (ER320LR) * Note:For additional technical information contact the ESAB Filler Metals Marketing Department