19 Typical Undiluted Type Weld Metal Analysis Specifications % wt Arcaloy ER316L AWS A5.9 Carbon 0.02 ASME SFA 5.9 Manganese 1.8 Class ER316/316L Silicon 0.4 MIL-19933 Chromium 19.0 MIL-316L Nickel 13.3 ABS-ER316/316L Molybdenum 2.2 FN 3 For  welding type 316 and 316L. Arcaloy ER316LSi AWS A5.9 Carbon 0.02 ASME SFA 5.9 Manganese 1.8 Class ER316Si/316LSi Silicon 0.8 Chromium 19.0 Nickel 13.3 Molybdenum 2.2 FN 6 Contains a higher amount of silicon, which markedly improves wetting characteristics for use in applications demanding a good cosmetic appearance. Recommended Welding Parameters page 21 Additional Stainless Cored Wires listed on page 20
Electrodes
Covered
Stainless
Steel
Products
Solid Wire
& Rod
Products
ESAB
TIG & MIG
Wires
Cored
Wire
Products
Submerged
Arc
Products
Hard-
surfacing
Products
Calculations
Filler Metals
ASTM
Steels
Conversion
Tables
Arcaloy SS
Electrode Coat.
Arcaloy
Bare Wires
Arcaloy Metal
Core Wires
Nickel-Arc/
Nicore Cast Iron
Shield-Bright
Gas/Flux Cored
Core-Bright
Cored Wires