36 Atom Arc 7018-1 AWS Class E7018-1 AC-DCEP (Electrode Positive) Electrode Imprint Marking:  7018-1 Code and Specification Data: AWS A5.1, ASME SFA 5.1 Det Norske Veritas - 3Y(H10) ABS - AWS A5.1, 3-3YHH CWB-CSA W48.1, E48018-1 Lloyds - 3-3YH

Description:

Atom Arc 7018-1 is an all-position, low hydrogen, iron powder electrode that displays exceptional impacts at low temperatures in both the as welded and stress relieved conditions. It more than meets the AWS minimum of 20 ft.-lbs. (27 J) at -50°F (-10°C). The smooth metal transfer minimizes spatter and the complete slag coverage is designed for easy removal. Atom Arc 7018-1 is intended for a wide variety of carbon and low alloy steels in the 50 ksi (345 MPa) minimum yield. It is ideal for applications that require impact toughness at low temperatures.
Covered
Electrodes
Stainless
Steel
Products
Solid Wire
& Rod
Products
ESAB
TIG & MIG
Wires
Cored
Wire
Products
Submerged
Arc
Products
Hard-
surfacing
Products
Calculations
Filler Metals
ASTM
Steels
Conversion
Tables
Electrode
Selection
A5.1 Mild Steel
Electrodes
Atom Arc Iron
Powder
A5.5 Low Alloy
Steel Elect