COPYRIGHT 2000 THE ESAB GROUP, INC. LESSON
III 3.7.3
SUREWELD
810P (AWS
E8010-P1)
- An all-position cellulosic electrode espe-
cially suited for welding high strength
pipe. It produces the consistent, deep penetration
required to maintain a proper keyhole
when vertical-down welding in open root pipe joints. X-
ray quality welds can be produced using
flat, horizontal, overhead, vertical-up, and vertical- down
procedures. Recommended for X60, X65, and X70 grade pipe.
Typical mechanical properties are:
Yield Strength - 72,700 psi
Tensile Strength - 88,300 psi
Elongation (2" Gauge) - 24%
Charpy V-Notch Impact Resistance
- 31 ft-lbs
@ -20°F 25
ft-lbs @ -50°F The
typical chemical composition of the weld metal is: Carbon
0.10% Sulfur
0.014% Manganese
0.48% Nickel
0.98% Silicon
0.24% Molybdenum
0.11% Phosphorus
0.008% DEPOSITION
RATE DATA:
SUREWELD 810P*
Electrode Deposition
Diameter
Amperage
Efficiency,
% (Lbs/Hr.)
3/32" 70
72.0% 1.5
100 65.0%
1.7 1/8"
100 76.34
2.12 130
68.81 2.31
5/32" 140
73.57 2.8
170 64.14
2.93 3/16"
160 74.9
3.3 190
69.7 3.52
*Note: Efficiencies do not include
stub loss