© COPYRIGHT 2000 THE ESAB GROUP, INC.
LESSON X
Specification No.
Description
A5.17-89
Carbon Steel Electrodes & Fluxes for Submerged Arc
Welding
A5.18-93
Carbon Steel Filler Metals for Shielded Arc Welding
A5.19-93
Magnesium Alloy Welding Rods & Bare Electrodes
A5.20-95
Carbon Steel Electrodes for Flux Cored Arc Welding
A5.21-80
Composite Surfacing Welding Rods & Electrodes
A5.22-95
Flux Cored Corrosion Resistant Chromium &
Chromium-Nickel Steel Electrodes
A5.23-90
Low Alloy Steel Electrodes & Fluxes for Submerged Arc
Welding
A5.24-90
Zirconium & Zirconium Alloy Bare Welding Rods &
Electrodes
A5.25-91
Consumables for Electroslag Welding of Carbon & High
Strength Low Alloy Steels
A5.26-91
Consumables for Electrogas Welding of Carbon & High
Strength Low Alloy Steels
A5.27-85
Copper and Copper Alloy Rods for Oxyfuel Gas Welding
A5.28-96
Low Alloy Steel Filler Metals for Gas Shielded Arc
Welding
A5.29-98
Low Alloy Steel Electrodes for Flux Cored Arc Welding
A5.30-79
Consumable Inserts
A5.31-92
Fluxes for Brazing and Braze Welding
10.3.1.1
These filler metal specifications also describe the classification requirements
concerning standardization such as electrode size and length, packaging, spooling, mark-
ing, labeling, and others.
10.3.2
AWS Structural Welding Code - Steel
-
The AWS Structural Welding Code -
Steel (AWS D1.1-96) covers the welding requirements applicable to welded steel structures
including buildings, bridges, and structures consisting of tubular shaped members. Factors
such as the design of welded connections, workmanship, welding procedure, welding
operator qualification, and inspection requirements are covered in this code. Previous to
the 1994 issue of this code, it also specified the tensile strength, yield strength, elongation,
and impact requirements for the low alloy flux cored electrodes, since no AWS Filler Metal
Specification existed for these electrodes. It is required that the user (contractor or fabrica-
tor) conduct tests to show that the low alloy weld metal would meet the mechanical proper-
ties mentioned above per the code.
Lesson 1
The Basics of Arc Welding
Lesson 2
Common Electric
Arc Welding Processes
Lesson 3
Covered Electrodes for Welding
Mild Steels
Lesson 4
Covered Electrodes for Welding Low Alloy Steels
Lesson 5
Welding Filler Metals for Stainless Steels
Lesson 6
Carbon & Low Alloy
Steel Filler Metals -
GMAW,GTAW,SAW
Lesson 7
Flux Cored Arc Electrodes Carbon Low Alloy Steels
Lesson 8
Hardsurfacing Electrodes
Lesson 9
Estimating & Comparing Weld Metal Costs
Lesson 10
Reliability of Welding Filler Metals
Current
Chapter
Table of Contents
Go To Test
Print
Glossary
Search
Chapter
(Faster Download)
Turn Pages
Search
Document
(Slower Download)