6 Diameters and Recommended Amperages 3/32" (2.4mm)—50-75 1/8" (3.2mm)—80-120 5/32" (4.0mm)—100-140 Identification All-State® No. 275 SUPER printed on electrode coating and package. Packaging 3/32" (2.4mm) x 9" (225mm) in 2-lb. (.91 kg) and 5-lb. (2.27 kg) containers. Other sizes in 3-lb. (1.36 kg) and 10-lb. (4.54 kg) containers.