35 Diameters and Recommended Amperages 3/32" (2.4 mm)—70-100 amps 1/8" (3.2 mm)—100-140 amps 5/32" (4.0 mm)—140-190 amps 3/16" (4.8 mm)—190-240 amps Identification All-State 616 MEGA II printed on electrode coating and package. Packaging All sizes in 10 lb. tubes