25 Diameters
and Recommended Amperages 1/16"
(1.6mm)25-50 3/32"
(2.4mm)70-120 1/8"
(3.2mm)90-140 5/32"
(4.0mm)130-190 Identification
All-State Monoweld®
printed on electrode coating and package. Packaging
1/16" (1.6mm) in 1-lb. (.45 kg) and
5-lb. (2.27 kg) containers. All other sizes in 3-lb. (1.36 kg), 5-lb. (2.27 kg)
and 10-lb. (4.54
kg) containers. ALL-STATE
Monoweld® Typical
Application: I beam welding.