23 Procedures Clean weld area. When welding in extreme low temperatures, it is advisable to warm base metal to 60°F (16°C). A short arc must be maintained to produce quality deposits. Remove all slag from previous pass before applying additional passes. Diameters and Recommended Amperages 1/8" (3.2mm)—100-150 5/32" (4.0mm)—120-210 Identification All-State HY-10® printed on electrode coating and package. Packaging All sizes in 5-lb. (2.27 kg) and 10-lb. (4.54 kg) containers. ALL-STATE HY-10® Typical Application: Stabilizer arm repair.