21 Diameters
and Recommended Amperages 3/32"
(2.4mm)60-100 5/32" (4.0mm)130-210
1/8" (3.2mm)100-160
3/16" (4.8mm)200-280 Identification
All-State®
616 printed on electrode coating and package. Packaging
All sizes in 5-lb. (2.27 kg) and 10-lb.
(4.54 kg) containers. ALL-STATE®
616 Typical Application:
A versatile, easily machined electrode for low-alloy and
free machining steels. Also ideally
suited for: Enameling steels, cold rolled steel,
steels with a high sulphur content such as shafts.