19 Diameters and Recommended Amperages 3/32" (2.4mm)—40-80 1/8" (3.2mm)—80-130 5/32" (4.0mm)—110-160 Identification All-State Steelarc Plus® printed on electrode coating and package. Packaging All sizes in 5-lb. (2.7 kg) and 10-lb. (4.54 kg) containers. ALL-STATE Steelarc Plus® A general purpose maintenance and repair electrode for use with all mild steels. Typical Application: Structural mild steel joining.