14 All-State® No. 430 Paste Solder Low Temperature Silver Bearing Solder For Torch, Furnace, Induction or Soldering Iron Applications General Characteristics Same as previous except that No. 430 solder in mesh form has been premixed with an active flux extending its range of applications. Procedures When using on stainless steels, add 1 drop of Duzall flux to joint carrying paste before heating. Size 8-oz. (.23 kg) plastic jars. Identification All-State® 430 Paste Solder printed on package. Packaging 8-oz. (.23 kg) plastic jars. ALL-STATE® 430 Paste Solder Typical Application: Automobile radiator repair.