23
All-State
Silflo® 5
Typical Applications
Used where close fit-up cannot be maintained.
Joint clearance .001" to .004". Qualities
Nominal Chemical Composition
Phosphorus: 6.00% Silver:
5.00% Copper: Balance Solidus
1190°F
(643°C) Liquidus
1485°F
(807°C) Brazing
temperature range1300°-1500°F (704°-816°C)
Meets specificationsAWS A5.8
(BCuP-3), QQ-B 650 (FS-BCuP-3); MIL-B-7883 (B-CuP-3) Sizes
.050" (1.3mm) x 1/8" (3.2mm) x 18"
(450mm), 1/16" (1.6mm) Round x 36" (900mm), 1/8" (3.2mm) Square x 36"
(900mm). Additional sizes available
upon request. Identification
Light blue color on tip of rod. All-State
Silflo® 5 printed on package.
Packaging 36"
(900mm) in 10-lb. (4.54 kg) containers. 18" (450mm) in 1-lb. (.45 kg), 10-lb.
(4.54 kg) and 25-Ib. (11.34
kg) containers.