4 ALL-STATE® 13/13 FC Typical Application: Gear teeth build up. Sizes 1/8" (3.2mm) and 3/16" (4.8mm) x 18" (450mm) bare and flux coated Identification All-State® 13 or 13FC printed on package. Flux coated rods have a rose colored coating. Bare rods have dark blue color on tip of rod. Packaging Bare in 1-lb. (.45 kg) and 10-lb. (4.54 kg) containers. Flux coated in 1-lb. (.45 kg), 3-lb. (1.36 kg) and 10-lb. (4.54 kg) containers.