14
Diameters and Recommended Amperages
3/32" (2.4mm)40-80
1/8" (3.2mm)70-110
5/32" (4.0mm)100-140
3/16" (4.8mm)120-160
Identification
All-State®
8 printed on electrode coating and package. Packaging
3/32" (2.4mm) x 9" (225mm) in 5-lb.
(2.27 kg) containers. 1/8" (3.2mm) and 5/32" (4.0mm) in 5-lb. (2.27 kg) and
10-lb. (4.54 kg) containers. 3/16"
(4.8mm) in 10-lb. (4.54 kg) containers.
ALL-STATE®
8
Typical Application:
Correcting foundry defects.