10
Handi-Jig Heat-resistant
compoundinsulates and holds parts in position for welding. Dual purpose
asbestos-free. Use as
a heat dam and insulator to protect base metal from the effects of heat. Dough
like consistency adheres to
most surfaces making it ideal for use as a jigging fixture or insulator for parts
to be welded. Will not distort or
shrink when heated.