Diameters and Recommended Amperages 1/8" (3.2mm)—120-150 5/32" (4.0mm)—140-190 3/16" (4.8mm)—190-250 1/4" (6.4mm)—250-310 Identification All-State Roll Matrix® printed on electrode coating and package. Packaging All sizes in 3-lb. (1.36 kg) and 10-lb. (4.54 kg)containers.