2
Diameter and Recommended Amperages
3/32" (2.4 mm)150-240
1/8" (3.2 mm)225-350
5/32" (4.0 mm)250-400
3/16" (4.8 mm)300-500
1/4" (6.4 mm)440-530
Identification
All-State®
Chamfer printed on electrode coating and package. Packaging
3/32" (2.4mm) x 14" (350mm) in 5-lb.
(2.27 kg) and 44-lb. (19.96 kg) containers. 1/4" (6.4mm) x 18" (450mm) in
50-lb. (22.68 kg) containers. All other
sizes in 5-lb. (2.27 kg) and 50-lb. (22.68 kg) containers.
ALL-STATE®
Chamfer Rod Typical
Application: Metal arc gouging.